UNSW atomic layer deposition (ALD)



0
3360

For more information about ALD see https://pv-manufacturing.org/hot-topics-and-trends/atomic-layer-deposition/ This animation is an online educational resource developed for the https://pv-manufacturing.org/website by Jing Zhao, Daniel Chen, and Jack Colwell in a project headed by Associate Professor Bram Hoex. The project funding was provided by the Australian Centre for Advanced Photovoltaics (ACAP) under Grant “CGR3 - Development of online educational resources for PV manufacturing education” and the Faculty of Engineering of UNSW Sydney. More information about the A/Prof Bram Hoex’s research group